A study on the beta' and beta" formation kinetics in AA6063 using differential scanning calorimetry

J van de Langkruis, MS Vossenberg, WH Kool, S van der Zwaag

Research output: Contribution to journalArticleScientificpeer-review

3 Citations (Scopus)
Original languageUndefined/Unknown
Pages (from-to)408-413
Number of pages6
JournalJournal of Materials Engineering and Performance
Volumevol. 12
Issue numberNo. 4
Publication statusPublished - 2003